HIGHER QUALITY AND BETTER SERVICE TO GIVE BACK TO CUSTOMERS
Appearance | Milky white emulsion |
Solid content | ≥43% |
Viscosity | 15-17S (TU-#4 cup, 25℃) |
PH value | 6.0-7.0 |
Peel off strength | (printing color) 60% off |
Strength after crimping | no layer separation |
High temperature resistance after crimping (180hours @ 60℃) | no layer separation, no blistering |
Freezing resistance after crimping (180hours @ -18℃) | no layer separation, no foam |
Embossing | Available , no foam, no separation |
Instructions:
1. Please clean the glue roller and glue tank of the laminator before and after use.
2. This product has been adjusted properly according to the technical standards, please don’t add any solvent or mix with other product in using.
3. After the adhesive-coated film is pre- dry, it can be directly laminated with the paper. Then After 2 hours, it can transfer to next process if needed, Such as embossing, bronzing,bumping, etc.
4. the after-printed paper must be completely dry then to be laminated.
Packing: 50KG plastic drum
Shelf life: 8 months Please use it within the valid time.
Storage: In house, 5℃-30℃ Avoid direct sunlight exposure.
Please make sure your contact information is correct. Your message will be sent directly to the recipient(s) and will not be publicly displayed. We will never distribute or sell your personal information to third parties without your express permission.